Crossref DOIMemberCiteFactoropen accessissn
SJIF Impact Factor 8.659 | ISSN: 2582-3930
IJSREM Logo

International Journal of Scientific Research in Engineering and Management

(Gateway to Global Scholars - An International, Scholarly, Multi-Disciplinary, Open Access Journal)

Peer-Reviewed Journal Designed to Meet UGC's Quality Parameters

HomeCurrent IssuePast IssuesPay OnlineConferencesEditorial BoardAbout UsContact Us
IJSREM

Loading article...

Follow Us

  • Google Scholar
  • ResearchGate
  • Academia.edu
  • Mendeley
  • LinkedIn
  • Facebook
  • Instagram

Journal Policies

  • Peer Review Policy
  • Publication Ethics
  • Copyright Infringement
  • Refund & Cancellation Policy
  • Terms and Conditions
  • Privacy Policy

Journal Identifiers & Licenses

  • ISSN Verified: 2582-3930ISSN Verified: 2582-3930
  • Crossref DOI: 10.55041Crossref DOI: 10.55041
  • SJIF Ranking: 08.659SJIF Ranking: 08.659
  • Licensed under CC BY 4.0Licensed under CC BY 4.0
  • ISO Certification: 9001:2015ISO Certification: 9001:2015
  • Indexed & Cited In: Google ScholarIndexed & Cited In: Google Scholar

Contact Us

International Journal of Scientific Research in Engineering and Management (IJSREM)

#62/1, New No 7, 1st Cross, 2nd Main, Ganganagar, R T Nagar, Bangalore North, Bangalore, Karnataka, India – 560032
[email protected]+91 93911 67991
logos
logos
Working Hours

Mon – Sat: 9:00 AM – 6:00 PM

Sunday: 10:00 AM – 4:00 PM

+91 93911 67991

© 2026 IJSREM – International Journal of Scientific Research in Engineering and Management. This is an open-access journal. Articles are published under the Creative Commons Attribution (CC BY 4.0) License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

DisclaimerPrivacy PolicyTerms and Conditions
ArticlePeer ReviewedOpen AccessPlagiarism Passed
Paper ID:IJSREM68940

COMPARATIVE EXPERIMENTAL EVALUATION OF WATERPROOFING ADMIXTURES ON THE MECHANICAL AND DURABILITY PERFORMANCE OF M20 CONCRETE

Stream/Area:

-

Subject:

-

Paper ID:

IJSREM68940

Volume:

10 |

11 |

Nov 2026

Pages:

1-8

Publication Frequency:

Monthly (12 issues per year)

DOI
Digital Object Identifier
10.55041/IJSREM68940

License:International Journal of Scientific Research in Engineering and Management follows the Creative Commons Attribution 4.0 (CC BY 4.0) License, allowing free use and distribution with proper attribution.

Share this article:

Authors

DAMV

D. ARYA MAYUR VARMA

Department of Civil Engineering

Sanketika Vidya Parishad Engineering College, P.M. Palem, Visakhapatnam – 530041, Andhra Pradesh, India

Download Author Certificate

Mentors

KDC

K. DILEEP CHOWDARY

Department of Civil Engineering

Sanketika Vidya Parishad Engineering College, P.M. Palem, Visakhapatnam – 530041, Andhra Pradesh, India

Download Mentor Certificate

Author Services & Downloads

Full ArticlesAcceptance Certificate

Abstract

This study evaluates the influence of five waterproofing-admixture categories—naphthalene-, melamine-, lignosulfonate-, polymer- and stearate-based formulations—on the fresh, mechanical and durability properties of M20 concrete. The experimental programme covers slump at water–cement ratios of 0.55, 0.60 and 0.70; 7- and 28-day compressive, split-tensile and flexural strengths; modulus of elasticity; steady-flow water permeability; rapid chloride penetration; accelerated reinforcement-corrosion assessment; 90-day acid and sodium-chloride exposure; and drying shrinkage. Three dosage levels (DI, DII and DIII) were considered for each admixture family. At 28 days, stearate DIII achieved the highest compressive strength (36.11 MPa), flexural strength (4.73 MPa) and modulus of elasticity (2.94 × 10⁴ N/mm²). Ligno DIII produced the highest split-tensile strength (5.54 MPa). Naphthalene DIII had the lowest tabulated 28-day permeability coefficient (5.0140 × 10⁻¹¹ m/s), representing a 22.85% reduction relative to the control. Polymer DIII exhibited the lowest reported corrosion-related steel mass loss (2.32%). The lowest shrinkage values varied with age: stearate DIII at 28 days and melamine DIII at 60 and 90 days. These results indicate that admixture performance is property-dependent. Interpretation is subject to uncertainties in dosage records, permeability data, RCPT reporting and exposure-test details; the reported findings therefore require confirmation against laboratory records.

KEYWORDS

Waterproofing admixtures M20 concrete compressive strength permeability chloride penetration corrosion drying shrinkage concrete durability.

Cite This Article

D. ARYA MAYUR VARMA, K. DILEEP CHOWDARY, "COMPARATIVE EXPERIMENTAL EVALUATION OF WATERPROOFING ADMIXTURES ON THE MECHANICAL AND DURABILITY PERFORMANCE OF M20 CONCRETE," International Journal of Scientific Research in Engineering and Management, vol. 10, no. 11, pp. 1-8, Nov 2026. https://doi.org/10.55041/IJSREM68940

Full Article/Conclusion

The experimental comparison of five waterproofing-admixture families in M20 concrete demonstrates that their influence varies across fresh, mechanical and durability properties. Within the limits of the reported test programme, the following conclusions are drawn: 1.      Slump generally increased with admixture dosage. Melamine-based admixture showed the greatest reported workability at the lower water–cement ratio, although unusually high slump readings require verification. 2.      Stearate DIII achieved the highest reported 28-day compressive strength (36.11 MPa), flexural strength (4.73 MPa) and modulus of elasticity (2.94 × 10⁴ N/mm²). 3.      Ligno DIII produced the highest reported 28-day split-tensile strength (5.54 MPa), confirming that the optimum admixture varied with the mechanical property considered. 4.      Naphthalene DIII had the lowest tabulated 28-day water-permeability coefficient (5.0140 × 10⁻¹¹ m/s), approximately 22.85% below the control value. This result should be interpreted after reconciling the conflicting permeability records. 5.      Polymer DIII produced the lowest reported embedded-steel mass loss (2.32%) in the accelerated-corrosion comparison, compared with 3.30% for the control concrete. 6.      Stearate DIII showed the lowest reported mass loss during acid and sodium-chloride exposure. Melamine DIII had the lowest reported shrinkage at 60 and 90 days, while stearate DIII had the lowest value at 28 days. 7.      The results support property-specific admixture selection rather than a universal ranking. Confirmation of dosage, permeability, RCPT and chemical-exposure records, together with independent replication, is necessary before the findings are used in specifications or design.

References

[1] ASTM C469-02, Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression, ASTM International, 2002. [2] L. K. Agarwal, “Waterproofing of buildings—Requirements, trends and guidelines,” CE and CR, vol. 14, no. 9, pp. 14–22, 2001. [3] E. Asakura, H. Yoshida, and H. Nakae, “Influence of superplasticizer on fluidity of fresh cement paste with different clinker phase composition,” in Proc. 9th Int. Congr. Chem. Cements, New Delhi, India, 1992, pp. 570–570. [4] K. K. Asthana and R. Lakhani, “Waterproofing in buildings—Problems and solutions,” NBM & CW, pp. 8–11, 2003. [5] A. O. Ata and M. O’Neill, “The physicochemical interaction between polymer slurry and cement mortar,” Geotechnical Testing Journal, vol. 23, pp. 225–235, 2000. [6] J. Bensted, “Early hydration behaviour of Portland cement in water, calcium chloride and calcium formate solutions,” Silicates Industriels, vol. 45, pp. 5–10, 1980. [7] S. Chandra and P. Flodin, “Interactions of polymers and organic admixtures on Portland cement hydration,” Cement and Concrete Research, vol. 17, pp. 875–890, 1987. [8] P. C. Chowdhry, “Strategies for resisting corrosion of reinforcement in concrete,” Indian Concrete Journal, 2004. [9] M. Collepardi, M. Corradi, and G. Baldini, “Hydration of C3A in the presence of lignosulfonate-carbonate system or sulfonated naphthalene polymer,” in Proc. 7th Int. Congr. Chem. Cements, Paris, 1980. [10] M. Collepardi, M. Corradi, and M. Valente, “Superplasticized shrinkage compensating concrete,” ACI SP-68, pp. 159–172, 1982.

Editorial & Review Transparency

Publication Date

11/13/2026

Peer Review Type

Double-Blind Peer Review

Review Rounds: 2

Documents

Review Report (Confidential)
Copyright Form (Office)

Article Metrics & Impact

Article Views

0

Total views since publication

PDF Downloads

2

Total downloads since publication

Geographic Reach

5

Indexing, Archiving & Preservation

Google Scholar
Academia
ResearchGate
Crossref
SSRN
Semantic Scholar
Thomson Reuters
WorldCat
Mendeley
OpenAlex
EBSCO
Zenodo

Digital Preservation: This article is permanently archived on Zenodo and complies with all data preservation standards across major indexing platforms.

Ethics, Compliance & Transparency

Plagiarism Screening

This manuscript has been checked for plagiarism using TurnitinPlagiarismChecker software.

Conflict of Interest

The authors declare no conflict of interest related to this research work.

Funding Information

No funding information available for this research.

Similar & Recommended Articles

Similar Articles by Topic

Related research in the same subject area

Loading similar articles...